Structur al Char acter istics of Laser - welded Cast Pur e Titanium Joints by Differ ent Gap Distance

ZHU Juan- fang1, HE Hui- ming2, LIU Fang3, ZHANG Chun- bao2, WANG Zhong- yi2   

  1. 1. Dept. of Stomatology, The First Affiliated Hospital of Zhengzhou University, Zhengzhou 450002, China; 2. Dept. of Prosthodontics, College of Stomatology, The Fourth Military Medical University, Xi′an 710032, China; 3. Legal Medical Clinic, Branch Office of Public Security Bureau, Pingdingshan 467000, China
  • Received:2006-12-25 Revised:2006-12-25 Online:2006-12-20 Published:2006-12-20
  • Contact: HE Hui- ming,Tel:029- 84776126

Abstract:

Objective To measure the microstructure of laser- welded cast pure titanium by different gap distance. Methods Forty specimens were sectioned and welded at four gap(s 0.00 mm, 0.25 mm, 0.50 mm and 1.00 mm). Took microhardness test and metallographic examination of welded zone surface. Results There were no difference in microhardness value and metallographic observation between welded specimens. The width of heat - effected zone was different. The smaller grains and needle- like αmartensitic structure were found in the heat- affected zone. Conclusion The effects of the joint gap were not significant.

Key words: titanium, laser- welding, structure