华西口腔医学杂志

• 专栏论著 • 上一篇    下一篇

多次烧结对Cercon饰面瓷磨损特性的影响

高清平1 巢永烈2 翦新春1 郭峰1   

  1. 1.中南大学湘雅医院口腔修复科, 湖南长沙410008;2.四川大学华西口腔医院口腔修复科, 四川成都610041
  • 收稿日期:2010-04-25 修回日期:2010-04-25 出版日期:2010-04-20 发布日期:2010-04-20
  • 通讯作者: 巢永烈,Tel:028-85503570
  • 作者简介:高清平(1972—),女,湖南人,副教授,博士
  • 基金资助:

    湖南省科技厅基金资助项目(2009JT3046)

Influence of multiple sintering on wear behavior of Cercon vene ering ceramic

GAO Qing -ping1, CHAO Yong-lie2, JIAN Xin-chun1, GUO Feng   

  1. 1. Dept. of Prosthodontics, Xiangya Hospital, Central South University, Changsha 410008, China; 2. Dept. of Prosthodontics, West China College of Stomatology, Sichuan University, Chengdu 610041, China
  • Received:2010-04-25 Revised:2010-04-25 Online:2010-04-20 Published:2010-04-20
  • Contact: CHAO Yong-lie,Tel:028-85503570

摘要:

目的探讨多次烧结对Cercon全瓷饰面瓷磨损性能的影响。方法采用体外实验模拟口腔环境,观察多次烧结后Cercon饰面瓷的磨损行为。实验中测量磨斑宽度以比较磨斑大小;采用扫描电镜(SEM)和原子力显微镜(AFM)观察磨斑形貌。结果随着烧结次数的增加,Cercon饰面瓷磨斑增大;磨斑宽度和烧结次数间存在着正相关(P<0.01);磨斑差异具有统计学意义(P<0.05)。SEM和AFM观察结果发现,随着烧结次数增多,犁沟减少,组织缺隙明显。结论多次烧结可以降低Cercon全瓷饰面瓷抗磨损性能,磨损模式有向严重磨损发展的趋势。

关键词: 磨损, 饰面瓷, 烧结

Abstract:

Objective To investigate the influence of multiple sintering on wear behavior of Cercon veneering ceramic. Methods Samples were fabricated according to the manufacture′s requirement for different sintering times (1, 3, 5, 7 times). The wear test was operated with a modified MM-200 friction and wear machine in vitro. The wear scars were characterized by scanning electron microscope(SEM) and atomic force microscopy(AFM). Results With the sintering times increasing, the wear scar width became larger. The correlation was significant at the 0.01 level. Significant difference was observed in wear scar width among different samples(P<0.05). SEM and AFM results showed that veneering ceramic wear facets demonstrated grooves characteristic of abrasive wear. Conclusion Multiple sintering can decrease the wear ability of Cercon veneer, and the wear pattern has the tendency to severe wear.