华西口腔医学杂志

• 专栏论著 • 上一篇    下一篇

纳米二氧化硅含量对硼酸铝晶须-二氧化硅熔附体填料复合树脂弯曲性能的影响

张文云1 袁艳波1 陈庆华2 肖玉鸿1 李星星1   

  1. 1.解放军昆明总医院·昆明医学院教学医院口腔科, 昆明650032;2.昆明理工大学材料与冶金工程学院, 昆明650093
  • 收稿日期:2011-04-25 修回日期:2011-04-25 出版日期:2011-04-20 发布日期:2011-04-20
  • 通讯作者: 张文云,Tel:0871-4774928
  • 作者简介:张文云(1970—),男,山西人,主任医师,博士
  • 基金资助:

    云南省自然科学基金资助项目(2004C0057M)

Influence of nano -silica content on flexural properties of the aluminum borate whisker and silica filler composite resins

ZHANG Wen-yun1, YUAN Yan -bo1, CHEN Qing -hua2, XIAO Yu -hong1, LI Xing -xing1   

  1. 1. Dept. of Stomatology, Kunming General Hospital of PLA; Teaching Hospital of Kunming Medical College, Kunming 650032, China; 2. Faculty of Materials and Metallurgical Engineering, Kunming University of Science and Technology, Kunming 650093, China
  • Received:2011-04-25 Revised:2011-04-25 Online:2011-04-20 Published:2011-04-20
  • Contact: ZHANG Wen-yun,Tel:0871-4774928

摘要:

目的研究正硅酸乙酯(TEOS)水解所得纳米二氧化硅(SiO2)含量对硼酸铝晶须(AlBw)与SiO2熔附体填料复合树脂弯曲性能的影响。方法采用TEOS溶胶-凝胶法制得纳米SiO2,按不同比例通过高温烧结使其熔附于AlBw表面,制作试样并测试其弯曲强度和弯曲弹性模量;利用透射电镜(TEM)观察高温处理过程对晶须表面形态的影响以及不同比例的熔附体形貌。结果AlBw-SiO2熔附体复合填料可显著提高牙科复合树脂的弯曲性能;AlBw和SiO2的质量比为3∶1时牙科复合树脂的弯曲强度达(130.29±8.38)MPa。结论TEOS溶胶-凝胶法水解所得的纳米SiO2含量可改善AlBw-SiO2熔附体填料复合树脂的弯曲性能。

关键词: 纳米二氧化硅, 晶须, 复合树脂, 弯曲性能

Abstract:

Objective To discuss the influence of nano-silica content which was hydrolyzed by tetraethyl orthosioate(TEOS) on the aluminum borate whisker(AlBw) and silica filler composite resins on flexural properties. Methods The nanometer-size silicon dioxide(SiO2) particles were prepared by sol-gel method based on tetraethyl orthosioate. Different proportion of AlBw and SiO2 were fused and attached onto the surface of AlBw through high temperature, then polymerized with resin matrix after surface siliconization and their flexural strength and flexural modulus were determined. The effects of heat treatment to the surface morphology of AlBw and the shapes of the mixture at various proportions were characterized by TEM. Results The flexural properties of dental composite resins with AlBw-SiO2 compound as inorganic fillers were significantly improved. The flexural property of a new type of dental composite resins was(130.29±8.38)MPa, when the mass ratio of AlBw and nano-SiO2 particle was 3∶1. Conclusion Nano-silica content which was hydrolyzed by tetraethyl orthosioate improved flexural properties of the aluminum borate whisker and silica filler composite resins.