[1] |
Costa-Palau S, Torrents-Nicolas J, Brufau-de Barberà M , et al. Use of polyetheretherketone in the fabrication of a maxillary obturator prosjournal: a clinical report[J]. J Prosthet Dent, 2014,112(3):680-682.
|
[2] |
Zoidis P, Papathanasiou I, Polyzois G . The use of a modified poly-ether-ether-ketone (PEEK) as an alternative framework material for removable dental prostheses. A clinical report[J]. J Prosthodont, 2016,25(7):580-584.
|
[3] |
Bayer S, Komor N, Kramer A , et al. Retention force of plastic clips on implant bars: a randomized controlled trial[J]. Clin Oral Implants Res, 2012,23(12):1377-1384.
|
[4] |
Stawarczyk B, Beuer F, Wimmer T , et al. Polyetheretherketone—a suitable material for fixed dental prostheses[J]. J Biomed Mater Res Part B Appl Biomater, 2013,101(7):1209-1216.
|
[5] |
Schmidlin PR, Stawarczyk B, Wieland M , et al. Effect of different surface pre-treatments and luting materials on shear bond strength to PEEK[J]. Dent Mater, 2010,26(6):553-559.
|
[6] |
Caglar I, Ates SM, Yesil Duymus Z . An in vitro evaluation of the effect of various adhesives and surface treatments on bond strength of resin cement to polyetheretherketone[J]. J Prosthodont, 2019,28(1):e342-e349.
|
[7] |
Uhrenbacher J, Schmidlin PR, Keul C , et al. The effect of surface modification on the retention strength of polyetheretherketone crowns adhesively bonded to dentin abutments[J]. J Prosthet Dent, 2014,112(6):1489-1497.
|
[8] |
Zhou L, Qian Y, Zhu Y , et al. The effect of different surface treatments on the bond strength of PEEK composite materials[J]. Dent Mater, 2014,30(8):e209-e215.
|
[9] |
熊芳 . 喷砂对全瓷底层材料的作用[D]. 成都: 四川大学, 2003.
|
|
Xiong F . The effect of sandblasting on all ceramic bottom material[D]. Chengdu: Sichuan University, 2003.
|
[10] |
翟建明 . 金属材料经硫化氢腐蚀后的疲劳可靠性研究[D]. 北京: 北京工业大学, 2013.
|
|
Zhai JM . Study of fatigue reliability on H2S corroded metallic materials[D]. Beijing: Beijing University of Technology, 2013.
|
[11] |
Vogel D, Dempwolf H, Baumann A , et al. Characterization of thick titanium plasma spray coatings on PEEK materials used for medical implants and the influence on the mechanical properties[J]. J Mech Behav Biomed Mater, 2018,77:600-608.
|
[12] |
Schwitalla AD, Spintig T, Kallage I , et al. Flexural behavior of PEEK materials for dental application[J]. Dent Mater, 2015,31(11):1377-1384.
|
[13] |
John J, Gangadhar SA, Shah I . Flexural strength of heat-polymerized polymethyl methacrylate denture resin reinforced with glass, aramid, or nylon fibers[J]. J Prosthet Dent, 2001,86(4):424-427.
|
[14] |
冯益华 . 新型陶瓷喷砂嘴的研究开发及其冲蚀磨损机理研究[D]. 济南: 山东大学, 2003.
|
|
Feng YH . Development of new ceramic nozzles and study on it’s erosion wear mechanisms[D]. Jinan: Shandong University, 2003.
|
[15] |
Tilly GP, Sage W . The interaction of particle and material behaviour in erosion processes[J]. Wear, 1970,16(6):447-465.
|
[16] |
董刚 . 材料冲蚀行为及机理研究[D]. 杭州: 浙江工业大学, 2004.
|
|
Dong G . Study on the erosion wear behaviors and mechanisms of several materials[D]. Hangzhou: Zhejiang University of Technology, 2004.
|
[17] |
林曦 . 酸蚀后钛表面理化性能研究[D]. 广州: 南方医科大学, 2014.
|
|
Lin X . Surface characteristics of titanium after acid etching[D]. Guangzhou: Nanfang Medical University, 2014.
|
[18] |
Posritong S, Borges AL, Chu TM , et al. The impact of hydrofluoric acid etching followed by unfilled resin on the biaxial strength of a glass-ceramic[J]. Dent Mater, 2013,29(11):e281-e290.
|
[19] |
Shibuya N, Porter RS . A kinetic study of PEEK sulfonation in concentrated sulfuric acid by ultraviolet-visible spectroscopy[J]. Polymer, 1994,35(15):3237-3242.
|
[20] |
Shu S, Kobayashi H, Okubo M , et al. Chemical anchoring of lauryl methacrylate-based reversed phase monolith to 1/16″ o.d. polyetheretherketone tubing[J]. J Chromatogr A, 2012,1242:59-66.
|
[21] |
张书香, 蒋圣俊, 李辉 , 等. 磺化聚醚醚酮膜的制备和性能研究进展[J]. 济南大学学报(自然科学版), 2009,23(1):42-46.
|
|
Zhang SX, Jiang SJ, Li H , et al. Development of preparation and application of sulfonated poly ether ether ketone[J]. J Jinan Univ (Sci Technol), 2009,23(1):42-46.
|
[22] |
Zaidi SMJ, Mikhailenko SD, Robertson GP , et al. Proton conducting composite membranes from polyetheretherketone and heteropolyacids for fuel cell applications[J]. J Membr Sci, 2000,173(1):17-34.
|