华西口腔医学杂志

• 基础研究 • 上一篇    下一篇

非贵金属烤瓷冠修复后牙龈组织和血液中镍铬元素含量分析

朱国威1,杨晓红1,陈丽娅2,陈 林1   

  1. 1.遵义医学院附属口腔医院 修复科,贵州 遵义563003;2.遵义市环保监测站,贵州 遵义563000
  • 收稿日期:2004-08-25 修回日期:2004-08-25 出版日期:2004-08-20 发布日期:2004-08-20
  • 通讯作者: 杨晓红,Tel: 0852-8635723
  • 作者简介:朱国威(1953-),男,安徽人,副教授,学士
  • 基金资助:

    贵州省科技厅自然科学基金资助项目(黔科字2001-309 号)

Analysis on Content of Ni-Cr in Gingival and Blood of Hares after Wearing Non-Noble Porcelain-Fused-to-Metal Crown

ZHUGuo-wei1,YANGXiao-hong1,CHENLi-ya2,CHENLing1   

  1. 1.Dept.ofProsthodontics,Zunyi Medical College,Zu- nyi563003,China; 2.Zunyi Environmental Monitoring Station,Zunyi563000,China
  • Received:2004-08-25 Revised:2004-08-25 Online:2004-08-20 Published:2004-08-20

摘要:

医学院附属口腔医院 修复科,贵州 遵义563003;2.遵义市环保监测站,贵州 遵义563000) [摘要] 目的 研究家兔前牙行非贵金属烤瓷冠修复后牙龈组织及血液中镍铬元素的含量,初步探讨产生牙龈灰线的原因。方法 选38只成年家兔为实验对象,备其上下前牙,用德国Vita非贵金属烤瓷合金制作烤瓷冠,粘固。 3个月及6个月后用石墨炉原子吸收光谱法对实验区龈组织和血液进行镍铬元素含量分析。结果 非贵金属烤瓷冠修复后6个月组的牙龈组织和血液中镍铬元素含量均比对照组及3个月组高(P<0.05)。3个月组的牙龈组织和血液中镍铬元素含量与对照组相比无差异(P>0.05)。结论 非贵金属烤瓷冠暴露于口腔环境中,并与牙龈组织及体液直接接触,其金属边缘很容易发生电化学腐蚀,造成金属离子游离于牙龈组织和血液中,一定时间后引起牙龈灰线。

关键词: 非贵金属烤瓷冠, 镍, 铬, 牙龈灰线, 电化学腐蚀

Abstract:

Objective Purpose of the studywas to investigate the content ofNickel(Ni) and Chromium(Cr) ion in gingival tis- sue and blood, and to discuss the reason of gray line in gingival afterwearing non-noble Porcelain-Fused-to-Metal crown.Methods  38 rabbits were selected as experimental animals which were divided into three groups: control group, group 1(3 months) and group 2( 6 months ). The content of Ni and Cr ion in gingival tissue and blood was detected by atomic absorption spectrometer. Results The amount of Ni and Cr in group 2 was significantly higher than that in other groups (P<0.05). There was no differ- ence between group 1 and control group (P>0.05).Conclusion The reason of gingival colouration might be the electrochemical corrosion. The metal ion was released in gingival tissue and blood.

Key words: non-noble porcelain-fused-to-metal crown, nickel, chromium, gray line, electrochemical corrosion