Physical properties of Au-Pt ceramic alloy after recasting

Cheng Hui1, Yang Song1, Li Xiurong2, Wu Weiqing3, Zheng Ming1, Wang Yinghui1.   

  1. 1. Dept. of Prosthodontics, Affiliated Stomatological Hospital, Fujian Medical University, Fuzhou 350002, China; 2. Dental Tech. Center, Affiliated Stomatological Hospital, Fujian Medical University, Fuzhou 350002, China; 3. Test Center, Fuzhou University, Fuzhou 350002, China
  • Online:2013-08-01 Published:2013-08-01

Abstract:

 Objective  To investigate the influences of recasting on the mechanical properties of Au-Pt ceramic alloy. Methods  Au-Pt ceramic alloy samples were prepared and recast for 3 times without adding any new Au-Pt ceramic alloy. The tensile strength, 0.2% yield strength, percentage of elongation, flexural strength,  flexural modulus and Vickers hardness of each specimen were measured. Results  Being cast for different times, the Au-Pt ceramic alloy showed no significant differences on their tensile strength, 0.2% yield strength, percentage of elongation, flexural strength or Vickers hardness. The flexural modulus of the Au-Pt alloys being cast for 2 or 3 times was significantly higher than that of the alloys being cast for 1 time(P<0.05). Conclusion  Au-Pt ceramic alloy can be recast for 3 times at least, without any decrease in the mechanical properties.

Key words: Au-Pt ceramic alloy, recast, physical properties